Slow-crack-growth and indentation damage in calcium magnesium aluminosilicate (CMAS) glass from desert sand 期刊论文
发表期刊: CERAMICS INTERNATIONAL. 出版年: 2018, 卷号: 44, 期号: 3, 页码: 2676-2682
作者:  Kedir, Nesredin;  Faucett, David C.;  Choi, Sung R.;  Bansal, Narottam P.
收藏  |  浏览/下载:17/0  |  提交时间:2019/11/29
CMAS (calcium magnesium aluminosilicate)  CMAS glass  Slow crack growth  Mechanical properties  Indentation fracture  Indentation deformation  