Knowledge Resource Center for Ecological Environment in Arid Area
DOI | 10.1016/S1006-706X(13)60086-2 |
Crevice Corrosion of K60 in Dry Desertification Saline Soil | |
Li Ming; Shi Zhimin; Liu Yubao | |
来源期刊 | Journal of Iron and Steel Research,International
![]() |
ISSN | 1006-706X |
出版年 | 2013 |
卷号 | 20期号:4页码:76-80 |
英文摘要 | Corrosion products of K60 crevice samples which were buried in Ordos area were analyzed by scanning electron microscopy and X-ray diffraction. The result showed that, the corrosion potential decreased differently in the crevice and a maximum negative existed at the bottom side; with pH value reduced, the dissolved oxygen was nearly exhausted in the crevice. When the opening side of the coupons was coupled with each other, the crevice corrosion in the crevice might be accelerated and the pH value gradually reduced; however, the oxygen was not completely exhausted. The unbalanced current density between anode and cathode was the main cause of blocked self-catalysis effect in the crevice, and was also the main cause of corrosion of alloys. Lumpy corrosion happened on the surface of metal, and rusty layer was composed of Fe_3O_4, Fe_2O_3, FeO, FeOOH and FeS which distributed in the opening of crevice. There were the reddish-brown corrosion products and white matter which distributed in the form of filiform and spotted in the center part of crevice. The analysis showed that the white matter might include oxide of Fe and NaHCO_3. |
英文关键词 | K60 crevice sample Ordos soil corrosion product |
类型 | Article |
语种 | 英语 |
收录类别 | CSCD |
WOS研究方向 | Metallurgy & Metallurgical Engineering |
CSCD记录号 | CSCD:4807808 |
资源类型 | 期刊论文 |
条目标识符 | http://119.78.100.177/qdio/handle/2XILL650/335197 |
作者单位 | Li Ming, Inner Mongolia University of Technology, Hohhot, Inner Mongolia 010051, China.; Shi Zhimin, Inner Mongolia University of Technology, Hohhot, Inner Mongolia 010051, China.; Liu Yubao, Baotou Research Institute of Rare Earths, Baotou, Inner Mongolia 014030, China. |
推荐引用方式 GB/T 7714 | Li Ming,Shi Zhimin,Liu Yubao. Crevice Corrosion of K60 in Dry Desertification Saline Soil[J],2013,20(4):76-80. |
APA | Li Ming,Shi Zhimin,&Liu Yubao.(2013).Crevice Corrosion of K60 in Dry Desertification Saline Soil.Journal of Iron and Steel Research,International,20(4),76-80. |